MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total 4180 Polypropylene, Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4180 polypropylene is an impact copolymer with an extra low melt flow. ATOFINA 4180 polypropylene has a very low fluidity providing good melt strength with exceptional impact properties.

Application

ATOFINA 4180 is designed to be particularly suited for pipe and sheet extrusion, blow molding and corrugated cardboard manufacture.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 0.70 g/10 min0.70 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.9 MPa3900 psi
Elongation at Yield 11 %11 %ASTM D638
Flexural Modulus 1.21 GPa175 ksiASTM D 790
Izod Impact, Notched NBNBASTM D256
 0.800 J/cm
@Temperature -20.0 °C
1.50 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched  1.00 J/cm²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
ASTM DIN53453
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM DIN53453
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FASTM D648
Vicat Softening Point 150 °C302 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
Total PPC 5660 Propylene, Heterophasic Copolymer
Total PPH 3825WZ Polypropylene, Injection Molding Grade
Total PSC 1540(AS) Crystal Polystyrene
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding

PFINAA063 / 38499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.