MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Rhenosin® W 759 Rubber Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Plasticizer to improve the low-temperature flexibility of elastomer vulcanizates

Application: Technical rubber components, e.g. automotive seals and gaskets, fuel pipes, wire and cable sheathing

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 - 1.05 g/cc0.0368 - 0.0379 lb/in³
Viscosity 20 - 35 cP20 - 35 cP
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.40e+8 ohm-cm1.40e+8 ohm-cm
Dielectric Constant 11.811.8
Dissipation Factor 0.5430.543
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 150 °C>= 302 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.44 - 1.461.44 - 1.46
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Appearanceslightly yellowish liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchcast™ 5400 Electrical Powder Resin
TIMCAL ENSACO™ 260G Conductive Carbon Black
3M Scotchcast™ 4 Electrical Insulating Resin
3M Scotchcast™ 265 Electrical Epoxy Powder Resin
Raschig Group DECAL® 5431 Phenolic

PLANY9050 / 209441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.