MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Ingeo 4043D can be converted into a biaxially oriented film with use temperatures up to 265ºF (130ºC). This film has excellent optics, good machinability and excellent twist and deadfold. These properties make 4043D film an ideal candidate for candy twist wrap and other packaging applications. Additional properties include advantageous barrier to flavor and grease and superior oil resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D1505
Moisture Vapor Transmission 13.8 - 15.7 cc-mm/m²-24hr-atm35.1 - 39.9 cc-mil/100 in²-24hr-atmASTM F1249
Oxygen Transmission 25.6 - 27.6 cc-mm/m²-24hr-atm65.0 - 70.1 cc-mil/100 in²-24hr-atmASTM D3985
Carbon Dioxide Transmission 106 - 118 cc-mm/m²-24hr-atm269 - 300 cc-mil/100 in²-24hr-atmNatureWorks test
Viscosity Measurement 4.0
@Temperature 30.0 °C
4.0
@Temperature 86.0 °F
Relative viscosity; 1.0 g/dl chloroform
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 410 °F
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 160 %160 %ASTM D882
Film Elongation at Break, TD 100 %100 %ASTM D882
Secant Modulus, MD 3.30 GPa479 ksiASTM D882
Secant Modulus, TD 3.900 GPa565.7 ksiASTM D882
Elmendorf Tear Strength, MD 0.591 g/micron15.0 g/milASTM D1922
Elmendorf Tear Strength, TD 0.512 g/micron13.0 g/milASTM D1922
Film Tensile Strength at Break, MD 110 MPa16000 psiASTM D882
Film Tensile Strength at Break, TD 145 MPa21000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 - 160 °C293 - 320 °FASTM D3418
Maximum Service Temperature, Air 130 °C266 °F
 
Optical PropertiesMetricEnglishComments
Haze 2.1 %2.1 %ASTM D1003
Gloss 90 %90 %20°; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Feed Temperature 180 °C356 °F
Adapter Temperature 200 °C392 °F
Die Temperature 200 °C392 °F
Melt Temperature 202 - 218 °C396 - 424 °F
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 4032D Film Grade PLA
Total Corbion Luminy L175 PLA, Biobased Polymer
NatureWorks® Ingeo™ 4060D Sealant Grade PLA
Overview of materials for Polylactic Acid (PLA) Biopolymer
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer

PNATU85a / 135569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.