MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Garlock 505 CPE Sheet Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: Style #505 is a branded, chlorinated polyethylene (CPE) sheet rubber product. CPE has excellent resistance to many chemical groups such as oils, acids, bases and alcohols. CPE is also very resistant to oxidation, heat and ozone.

Information provided by Garlock Rubber Technologies

Key Words: chlorinated polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65 - 7565 - 75
 80 - 90
@Treatment Temp. 125 °C,
Time 252000 sec
80 - 90
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
Tensile Strength >= 12.4 MPa>= 1800 psi
 13.8 MPa2000 psiTypical
Elongation at Break >= 350 %>= 350 %
 >= 300 %
@Treatment Temp. 125 °C,
Time 252000 sec
>= 300 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Compression Set 60 %
@Temperature 125 °C,
Time 79200 sec
60 %
@Temperature 257 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BorsodChem ONGRO CPE 3602 N Chlorinated Polyethylene
Aurora Plastics CPE-01-266LT Wire and Cable CPE
Ethylene Propylene Rubber (EPM, EPDM)
Avient FireCon™ CPE 30-11 REV 2 Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE 32-33 RoHS Black Polyethylene, Chlorinated (CPE)

PGARL989 / 157462

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.