MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASON™ P MT Polyphenylsulfone (PPSU)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well as exceptional resistance to repeated autoclave cycles. It is available in several colored and transparent grades, and is tested to the requirements of ISO 10993.

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Water Absorption 0.37 %
@Time 86400 sec
0.37 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 1.1 %1.1 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 123123ASTM D785
Tensile Strength, Yield 69.6 MPa10100 psiASTM D638
Elongation at Break 60 %60 %ASTM D638
Tensile Modulus 2.34 GPa340 ksiASTM D638
Flexural Strength 91.0 MPa13200 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Compressive Strength 98.94 MPa14350 psiASTM D695
Izod Impact, Unnotched 6.94 J/cm13.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.44
@Frequency 60 Hz
3.44
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 14.2 kV/mm360 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.6 µm/m-°C17.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 182 °C360 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 216 °C420 °FASTM D648
Vicat Softening Point 218 °C424 °FASTM D1525
Flammability, UL94 V-0V-0UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Ensinger TECASON™ P Polyphenylsulfone (PPSU)
Avient Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU)
Evonik Europlex® PPSU Polyphenylsulfone Engineering Plastic

PENSIN063 / 104754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.