MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

3M 6Ns Ultra High Purity Boron
Categories: Ceramic

Material Notes: Ceradyne, Inc., a 3M company, manufactures UHP boron products enriched in 11boron. These products are produced using a unique proprietary process that yields a high purity metallic product. The following general characteristics are applicable to UHP boron products. Some of these data are based on naturally-occurring boron and may not reflect other specific isotope concentrations.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.38 g/cc2.38 g/cc
Molecular Weight 10.99 g/mol10.99 g/mol
Surface Tension 1100 dynes/cm1100 dynes/cm
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 1111
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 460.48 GPa66787 ksiYoung's
Shear Modulus 235.14 GPa34104 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.80e+6 - 2.00e+6 ohm-cm1.80e+6 - 2.00e+6 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 27.2 W/m-K188 BTU-in/hr-ft²-°F
Melting Point 2200 - 2300 °C3990 - 4170 °F
Boiling Point 2550 °C4620 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 99.9999 %99.9999 %
 
Descriptive Properties
Hardness3300 kg/mm2Knoop-100 gram load
Impurities<0.01 ppmSb
 <0.01 ppmSe
 <0.01 ppmAg
 <0.01 ppmAs
 <0.01 ppmHg
 <0.02 ppmCO2
 <0.02 ppmGe
 <0.025 ppmMn
 <0.03 ppmPb
 <0.03 ppmSn
 <0.04 ppmBi
 <0.05 ppmNi
 <0.07 ppmGa
 <0.1 ppmCd
 <0.1 ppmLi
 <0.1 ppmCr
 <0.1 ppmCu
 <0.1 ppmBa
 <0.1 ppmSr
 <0.2 ppmAl
 <0.5 ppmMg
 <0.5 ppmZn
 <0.5 ppmP
 <0.5 ppmNa
 <0.7 ppmK
 <0.9 ppmCa
 <0.9 ppmFe
 <1 ppmSi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sinotek Materials Packing Carbon Fiber with Graphite
Sinotek Materials Packing Carbonized Fiber Braided
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
CeramTec Alunit® Aluminum Nitride
3M 4014 Damping Aluminum Foam Sheet

PMM40045 / 194936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.