System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Beijing Chemical Industry KAIFA® M105 MPPO Resin
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Ether/PPO
Material Notes:
Flame retardant, Thermal resistant
Information provided by Beijing Chemical Industry Research Institute (Group)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.08
g/cc
0.0390
lb/in³
ASTM D792
Water Absorption
0.10 %
0.10 %
24 hr; ASTM D570
Linear Mold Shrinkage
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
50.0
MPa
7250
psi
ASTM D638
Elongation at Break
30 %
30 %
ASTM D638
Flexural Strength
78.0
MPa
11300
psi
ASTM D790
Flexural Modulus
2.40
GPa
348
ksi
ASTM D790
Charpy Impact, Notched
1.50
J/cm²
7.14
ft-lb/in²
ISO179
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Dielectric Constant
2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength
22.0
kV/mm
@Thickness 2.00 mm
559
kV/in
@Thickness 0.0787 in
ASTM D149
Dissipation Factor
0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
ASTM D150
Thermal Properties
Metric
English
Comments
CTE, linear
70.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
38.9
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)
100
°C
212
°F
ASTM D648
Flammability, UL94
V-1
@Thickness 3.20 mm
V-1
@Thickness 0.126 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
260
°C
500
°F
Middle Barrel Temperature
280
°C
536
°F
Front Barrel Temperature
280
°C
536
°F
Nozzle Temperature
275
°C
527
°F
Mold Temperature
80.0
°C
176
°F
Injection Pressure
120
MPa
17400
psi
Cycle Time - Injection
35
sec
35
sec
Screw Speed
70
rpm
70
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO
Beijing Chemical Industry KAIFA® M106N MPPO Resin
Beijing Chemical Industry KAIFA® M106 MPPO Resin
Beijing Chemical Industry KAIFA® M105N MPPO Resin
Beijing Chemical Industry KAIFA® M104N MPPO Resin
PKAIF50 / 48632
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.