MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Supreme Petrochem SP 556 Flame Retardant Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: Characteristics
  • Good flow properties
  • Good balance of toughness and rigidity
  • Available in any color
Processing
  • Extrusion
  • Molding
Applications
  • T.V. Cabinets, computer monitor, printer housing
  • Electrical switch boards, MCB distribution boxes, electrical gang boxes
  • Extruded sheets can be used for lining in mass transit system and for forming appliances bodies
Material Status: Commercial : Active

Agency Ratings: FDA 21 CFR 177.1640, UL file E185934

Information provided by Supreme Petrochem LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
Melt Flow 4.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.5 MPa3990 psi50 mm/min; ASTM D638
Elongation at Break 30 %30 %50 mm/min; ASTM D638
Flexural Strength 37.2 MPa
@Thickness 3.20 mm
5400 psi
@Thickness 0.126 in
ASTM D790
Flexural Modulus 1.77 GPa
@Thickness 3.20 mm
256 ksi
@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 1.00 J/cm
@Thickness 3.20 mm
1.87 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 93
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 93
Dielectric Constant 2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
IEC 250
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 450 V450 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 82.0 °C180 °FIEC335-1
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °FASTM D648
Vicat Softening Point 103 °C217 °F1kg load; 120°C/h; ASTM D1525
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Test 960 °C1760 °FIEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 250 °C<= 482 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 60.0 - 80.0 °C140 - 176 °F( 2 hrs) Pre drying temp.
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Luranyl® KR 2404 Polyphenylene Ether + Styrene-Butadiene Blend
INEOS Styrolution PS 158 N/L GPPS
Supreme Petrochem SP 6460 High Heat Polystyrene
Daikin NEOFLON® EA-LR43 ETFE Pellets
Chemours Tefzel® 210 Resin Modified ETFE

PSUP14 / 69446

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.