MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Inno-Comp INNOPOL® CS 2-3110 TO BU 10% Talc Filled Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes: INNOPOL® CS 2-3110 TO BU is a 10% talc-filled, black colored and UV stabilized compound based on polypropylene block-copolymer.

INNOPOL® CS 2-3110 TO BU is developed for producing injection molded automotive components, where the required properties are the good stiffness and excellent impact resistance.

Information provided by INNO-COMP

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ISO 1183
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 g/10 min
@Load 4.76 lb,
Temperature 446 °F
nozzle diam 2.095 mm; ISO 1133
Storage Temperature <= 60.0 °C<= 140 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 22.0 MPa3190 psi50 mm/min; ISO 527-1,-2
Elongation at Yield 8.0 %8.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1.20 GPa174 ksi1 mm/min; ISO 527-1,-2
Flexural Modulus 1.25 GPa181 ksiISO 178
Charpy Impact, Notched  0.600 J/cm²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °FISO 75-1,-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 250 °C374 - 482 °FInjection
Middle Barrel Temperature 190 - 250 °C374 - 482 °FInjection
Front Barrel Temperature 190 - 250 °C374 - 482 °FInjection
Melt Temperature 210 - 260 °C410 - 500 °FInjection
Mold Temperature 10.0 - 50.0 °C50.0 - 122 °F
Moisture Content <= 0.070 %<= 0.070 %
 
Descriptive Properties
Resin DesignationPP/PE TD 10ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 10% Talc Filled
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene
A. Schulman Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Conditioned

PINNO908 / 150108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.