MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Series 100 Liquid Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: LUCITE® LIQUID ACRYLIC RESINS SERIES 100
For the manufacture of solid surface shapes
Ambient temperature cure
Can be used on batch or continuous in-line mixing equipment

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 180 - 450 cP
@Temperature 23.0 °C
180 - 450 cP
@Temperature 73.4 °F
Linear Mold Shrinkage 0.00040 cm/cm0.00040 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 6060Cured; BS 2782 Pt 10
Flexural Strength 60.0 MPa8700 psiBS EN ISO 178, Cured
Flexural Modulus 8.00 GPa1160 ksiBS EN ISO 178, Cured
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month9.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Chemical Sumipex® LG2 Acrylic Resin, High Flow
Lucite International Series 500 Liquid Acrylic Resin
Sumitomo Chemical Sumipex® LG Acrylic Resin, High Flow
Lucite International Lucite® 41 Acrylic Bead Resin
Lucite International Lucite® 30B Acrylic Bead Resin

PLUCIT9404 / 150118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.