MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baybond® PU 401 A Polyester Urethane Polymer
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Anionic/non-ionic polyester urethane polymer. As the film-forming component in glass fiber sizes.

Properties / Applications: Baybond® PU 401 A was developed for the sizing of glass fibers used to reinforce thermoplastics, particularly polyamide. Glass fiber sizes based on Baybond® PU 401 A are characterized by their outstanding film-forming properties and very good adhesion. They have high colorfastness, even at elevated temperatures. Baybond® PU 401 A is also very stable against shear forces.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³DIN EN ISO 2811/3
Volatiles 48 - 52 %48 - 52 %0.9-1.1g / 1h / 125°C, convection oven; DIN EN ISO 3251
pH 6.5 - 8.56.5 - 8.5DIN ISO 976

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baybond® PU 406 Polyurethane
Covestro Baybond® PU 402 A Polyester Urethane Polymer
Covestro Baybond® PU 330 Polyester Urethane Polymer
Covestro Baybond® PU 407 Polyester Urethane Polymer
Covestro Baybond® PU 130 Polyurethane Resin

PCOVEST0069 / 201852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.