MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) Tedur® L 9200-1 Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: 60% glass fiber/mineral. High toughness. Application: automotive, various, seals

Information provided by ALBIS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 150 MPa21800 psiISO 527-1/-2
Elongation at Break 1.4 %1.4 %ISO 527-1/-2
Tensile Modulus 17.0 GPa2470 ksiISO 527-1/-2
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Flexural Strain at Break 1.6 %1.6 %ISO 178
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eU
 3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FISO 75-1/-2
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Glow Wire Flammability Index  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
DIN EN 60695
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
DIN EN 60695
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 340 °C608 - 644 °Finjection molding
Mold Temperature <= 140 °C<= 284 °Finjection molding
Drying Temperature 130 - 140 °C
@Time 7200 - 14400 sec
266 - 284 °F
@Time 2.00 - 4.00 hour
in desiccant dryer, depends on moisture content
 
Descriptive Properties
Tracking Resistance225IEC 60112

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Barlog Plastics KEBATRON L1065X3 PPS, linear, 65% glass fiber / mineral reinforced
Celanese Fortron® 6165 A4 Polyphenylene Sulfide (PPS), 65% Mineral/Glass-Fiber
Avient Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
MOCOM (ALBIS) Tedur® L 9523 PPS, 60% Glass Fiber/Mineral
Asahi Kasei Xyron™ DG235 PPS/PPE

PALBIS9923 / 221019

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.