MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman BMC 310 Cosmetic and Appliance Grade Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.

Typical applications are oven handles, vent trim and control panels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 2.00 g/cc1.80 - 2.00 g/cc
Water Absorption 0.10 - 0.20 %0.10 - 0.20 %24 hours, 23°C
Linear Mold Shrinkage 0.0015 - 0.0040 cm/cm0.0015 - 0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 40 - 5540 - 55
Tensile Strength, Ultimate 34.5 - 55.2 MPa5000 - 8000 psi
Flexural Strength 68.9 - 124 MPa10000 - 18000 psi
Flexural Modulus 11.0 - 13.8 GPa1600 - 2000 ksi
Compressive Strength 124 - 152 MPa18000 - 22000 psi
Izod Impact, Notched 1.07 - 3.20 J/cm2.00 - 6.00 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C425 - 500 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC 304 Automotive Grade Molding Compound
Overview of materials for Thermoset Polyester Glass Filled BMC
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
A. Schulman BMC 300 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 1412 Flame and Track Resistant

PBMC005 / 27188

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.