MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec 447 Cordierite
Categories: Ceramic; Oxide; Aluminum Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as cost-effective extruded and dry-pressed forms. 447 offers excellent thermal shock resistance with high continuous porosity, suitable for applications such as welding tile.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 14 - 17 %14 - 17 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 280280HV 0.5; DINV ENV 843-4
Tensile Strength at Break 17.2 MPa2490 psiACMA Test #4 / DIN EN 843-1
Tensile Modulus 125 GPa18100 ksiYoung's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 23.4 MPa3390 psi20 x 40 mm
Compressive Strength 123 MPa17800 psiASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.200.20DINV ENV 843-2
Shear Modulus 50.0 GPa7250 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  700000 ohm-cm
@Temperature 900 °C
700000 ohm-cm
@Temperature 1650 °F
 4.90e+7 ohm-cm
@Temperature 500 °C
4.90e+7 ohm-cm
@Temperature 932 °F
 1.00e+13 ohm-cm
@Temperature 100 °C
1.00e+13 ohm-cm
@Temperature 212 °F
IEC 672-1
 1.00e+14 ohm-cm
@Temperature 25.0 °C
1.00e+14 ohm-cm
@Temperature 77.0 °F
ASTM-D257
Dielectric Constant 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Strength 2.362 kV/mm59.99 kV/in6.35 mm (1/4") IEC 672-1
Dissipation Factor 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
Dielectric Loss Index 0.048
@Frequency 1e+6 Hz
0.048
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.600 µm/m-°C
@Temperature 20.0 - 200 °C
0.333 µin/in-°F
@Temperature 68.0 - 392 °F
 1.50 µm/m-°C
@Temperature 20.0 - 600 °C
0.833 µin/in-°F
@Temperature 68.0 - 1110 °F
ASTM-C373
 1.70 µm/m-°C
@Temperature 20.0 - 1000 °C
0.944 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.700 J/g-°C
@Temperature 100 - 200 °C
0.167 BTU/lb-°F
@Temperature 212 - 392 °F
DINV ENV 821-3
Thermal Conductivity 1.70 W/m-K11.8 BTU-in/hr-ft²-°FDIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1100 °C2010 °F
 
Descriptive Properties
ColorBrown
Te Value (°C)850
Thermal Shock Resistance R1 (K)800Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2)
Advanced Ceramics ACL 2089 Cordierite
CeramTec 701 Cordierite
CeramTec Sikor® E Cordierite
Cordierite, 2MgO-2Al2O3-5SiO2

CCERA925 / 107525

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.