MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 223 Transparent, Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product Description: QSil 223 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity which allows for ease of flow around complex parts, providing electrical insulation and shock resistance. The chemical composition provides hydrolytic and reversion resistance.

Key Features:

  • Convenient 1:1 mixing ratio for use in automatic dispensing equipment or hand mixing
  • Contains no solvents
  • Non-yellowing catalyst system

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccUncatalyzed, QSil 223A
 1.03 g/cc1.03 g/ccUncatalyzed, QSil 223B
Viscosity 2400 cP2400 cPUncatalyzed, QSil 223B
 3200 cP3200 cPUncatalyzed, QSil 223A
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inCured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5151Cured 24 hours @ 25°C
 5353Cured 1 hour @ 70°C
 6565Cured 1 hour @ 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+15 ohm-cm1.70e+15 ohm-cm
Dielectric Constant 2.69
@Frequency 1000 Hz
2.69
@Frequency 1000 Hz
Dielectric Strength 19.7 kV/mm500 kV/in
Dissipation Factor 0.00060
@Frequency 1000 Hz
0.00060
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 275 µm/m-°C153 µin/in-°F
Specific Heat Capacity 0.700 J/g-°C0.167 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 HB
@Thickness 1.70 mm
HB
@Thickness 0.0669 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4051.405
Transmission, Visible >= 98 %
@Thickness 1.00 mm,
Wavelength 400 nm
>= 98 %
@Thickness 0.0394 in,
Wavelength 400 nm
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 70.0 °C
1.00 hour
@Temperature 158 °F
 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Gel Time 120 min120 minCatalyzed
 
Descriptive Properties
ColorClearUncatalyzed, QSil 223A
 ClearUncatalyzed, QSil 223B
 Clear, colorlessCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
CHT Group QSil 218 Transparent, Liquid Silicone Rubber
CHT Group QSil 219 Transparent, Liquid Silicone Rubber
CHT Group QSil 220 Transparent, Liquid Silicone Rubber
CHT Group QSil 229 Transparent, Liquid Silicone Rubber

PACC2086 / 199474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.