System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Sumitomo Bakelite SUMILITE® ALC-1371 CCL Material
Categories:
Polymer
Material Notes:
Aluminum Base CCL High heat releasing material for LED lighting , power modules, etc. It is supplied as sheet for printed wiring boards (PCB).
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Water Absorption
0.30 %
0.30 %
D-24/23
Mechanical Properties
Metric
English
Comments
Peel Strength
1.70
kN/m
9.70
pli
A; 35umCF
Electrical Properties
Metric
English
Comments
Volume Resistivity
2.70e+14
ohm-cm
2.70e+14
ohm-cm
C-96/40/90
1.20e+16
ohm-cm
1.20e+16
ohm-cm
A
Surface Resistance
2.60e+14
ohm
2.60e+14
ohm
C-96/40/90
3.00e+15
ohm
3.00e+15
ohm
A
Dielectric Constant
7.6
@Frequency 1e+6 Hz
7.6
@Frequency 1e+6 Hz
C-96/20/65
7.8
@Frequency 1e+6 Hz
7.8
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
Dissipation Factor
0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
C-96/20/65
0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
Comparative Tracking Index
600
V
600
V
A; IEC; Tracking Resistance
Thermal Properties
Metric
English
Comments
Thermal Conductivity
7.00
W/m-K
48.6
BTU-in/hr-ft²-°F
A; Laser Flash
Glass Transition Temp, Tg
130
°C
266
°F
10°C/min
130
°C
266
°F
5°C/min
Flammability, UL94
V-0
V-0
Flame Resistance
Descriptive Properties
Breakdown Voltage AC
5
A; 25mmf pattern
Breakdown Voltage DC
>10
A; 25mmf pattern
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Bakelite® PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Sumitomo Bakelite SUMILITE® PLC-2147 RH Paper Phenolic
Sumitomo Bakelite SUMILITE® PL-1147 Paper Phenolic Laminate
Sumitomo Bakelite SUMILITE® ELC-4765/EI-6765 Glass Epoxy Laminate
PSUMIT120 / 193925
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.