DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used unmodified and according to good manufacturing practices for food contact applications. It has been approved by USDA for packaging meat and poultry products. Film properties below based on a film thickness of 30 µm. Data provided by Dow Chemical. |