MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Avient Versaflex™ CL E95 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizers. New Product. Commercial specifications have not been established. - Flexible - Formulated without Plasticizers - High Clarity

Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carriers are most suitable for coloring Versaflex™ CL E95. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Drying is not Required. Rear Zone = 330-370F Center Zone = 350-400F Front Zone = 360-420F Screw Speed = 100-500 RPM

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.898 g/cc0.898 g/ccASTM D792
Oxygen Transmission 150 cc-mm/m²-24hr-atm
@Thickness 0.120 mm,
Temperature 21.0 °C
381 cc-mil/100 in²-24hr-atm
@Thickness 0.00472 in,
Temperature 69.8 °F
ASTM D3985
Oxygen Transmission Rate 1200 cc/m²/day
@Thickness 0.120 mm,
Temperature 21.0 °C
77.3 cc/100 in²/day
@Thickness 0.00472 in,
Temperature 69.8 °F
ASTM D3985
Viscosity  30000 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
30000 cP
@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
 138000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
138000 cP
@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 959510 sec; ASTM D2240
Tensile Strength at Break 17.2 MPa
@Temperature 23.0 °C
2490 psi
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress at Strain  11.6 MPa
@Strain 100 %,
Temperature 23.0 °C
1680 psi
@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
 11.9 MPa
@Strain 300 %,
Temperature 23.0 °C
1730 psi
@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 580 %
@Temperature 23.0 °C
580 %
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 126 kN/m719 pliASTM D624
Compression Set  38 %
@Temperature 22.0 °C,
Time 79200 sec
38 %
@Temperature 71.6 °F,
Time 22.0 hour
ASTM D395B
 66 %
@Temperature 70.0 °C,
Time 79200 sec
66 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 71 %
@Temperature 100 °C,
Time 79200 sec
71 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Die Temperature 171 - 199 °C340 - 390 °F
Melt Temperature 182 - 204 °C360 - 399 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1210
USP Class VI YesYes
 
Descriptive Properties
Agency RatingsISO 10993 Part 4
 ISO 10993 Part 5
AppearanceClear/Transparent
FeaturesGood Flexibility
 High Clarity
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesBottles
 Film
 Medical/Healthcare Applications
 Personal Care

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
Avient Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Avient Versaflex™ CL2242 Thermoplastic Elastomer (TPE)
Avient Versaflex™ HC MT317 Thermoplastic Elastomer (TPE)
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber

PH0POL1201 / 145770

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.