MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® T90 HT Polycarbonate + ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC+ABS)-Blend; high heat resistance; Vicat/B 120 temperature = 135 °C; easy flowing; ball indentation temperature >= 125 °C; suitable as supporting material for energized parts

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.70 %0.70 %ISO 62
Viscosity 250000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
250000 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
melt; b.o. ISO 11443-a
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 3.00 mm
0.0060 - 0.0080 in/in
@Thickness 0.118 in
150x105x3 mm; 260 °C / MT 80 °C; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 3.00 mm
0.0060 - 0.0080 in/in
@Thickness 0.118 in
150x105x3 mm; 260 °C / MT 80 °C; b.o. ISO 2577
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 260 °C
30 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psi50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 56.0 MPa8120 psi50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1/-2
Izod Impact, Notched (ISO)  21.0 kJ/m²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 44.0 kJ/m²
@Temperature 23.0 °C
20.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180-U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+17 ohm1.00e+17 ohmIEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0015
@Frequency 100 Hz
0.0015
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C264 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75-1,-2
Vicat Softening Point  133 °C
@Load 5.10 kg
271 °F
@Load 11.2 lb
50°C/h; ISO 306
 135 °C
@Load 5.10 kg
275 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.850 mm
HB
@Thickness 0.0335 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T65 HI PC/ABS Blend
Covestro Bayblend® T85 XF Polycarbonate + ABS
Covestro Bayblend® T88 GF-20 Polycarbonate + SAN Glass Filled Impact Grade
Covestro Bayblend® T65 PG PC/ABS Blend
Covestro Bayblend® T65 XF Polycarbonate + ABS

PB09742 / 92582

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.