MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYBATCH™ White P8555 SC Concentrate Based In Random Copolymer Polypropylene
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description

POLYBATCH® P8555 SC is a high quality white masterbatch containing 50% TiO2 based in random copolymer polypropylene. This product offers excellent dispersion and a very low moisture content which permits high temperature processing. POLYBATCH® P8555 SC is recommended for use in cast, blown, OPP, or BOPP film applications requiring high loading levels with optimum dispersion.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
Moisture Absorption <= 0.0600 %<= 0.0600 %ASTM D789
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 50 %50 %
 
Descriptive Properties
Pellet Count 24pellets/gram

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ White P8550 C Concentrate Based In Polypropylene
A. Schulman POLYBATCH™ White P8555 T2 Concentrate Based In Homopolymer Polypropylene
A. Schulman POLYBATCH™ White P8555 SD Concentrate Based In Homopolymer Polypropylene
A. Schulman POLYBATCH™ Poly White P80494PF Concentrate Based In Polypropylene
A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate

PASHU509 / 25473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.