System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD
Categories:
Polymer
;
Film
;
Thermoset
;
Silicone
Material Notes:
Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.
Information provided by Fujipoly Industries
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
2.51
g/cc
2.51
g/cc
70°C for 1,000 hrs; JIS-K-6220
2.52
g/cc
2.52
g/cc
60°C for 1,000 hrs with 90% RH; JIS-K-6220
2.56
g/cc
2.56
g/cc
50°C for 1,000 hrs; JIS-K-6220
2.60
g/cc
2.60
g/cc
JIS-K-6220; ASTM D-792
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
49
49
ASTM D2240
Tensile Strength, Yield
5.00
MPa
725
psi
150°C for 1,000 hrs; JIS-K-6251
6.00
MPa
870
psi
70°C for 1,000 hrs; JIS-K-6251
7.00
MPa
1020
psi
60°C for 1,000 hrs with 90% RH; JIS-K-6251
11.0
MPa
1600
psi
JIS-K-6251(#2)/ASTM D-412
Elongation at Yield
15 %
15 %
JIS-K-6251(#2)/ASTM D-412
15 %
15 %
70°C for 1,000 hrs; JIS-K-6251
Tear Strength
11.0
kN/m
62.8
pli
70°C for 1,000 hrs; JIS-K-6252
21.0
kN/m
120
pli
JIS-K-6252 (Angle)/ASTM D-624
Electrical Properties
Metric
English
Comments
Volume Resistivity
2.90e+13
ohm-cm
2.90e+13
ohm-cm
7.80e+13
ohm-cm
7.80e+13
ohm-cm
70°C for 1,000 hrs; JIS-K-6249
1.50e+14
ohm-cm
1.50e+14
ohm-cm
150°C for 1,000 hrs
1.50e+14
ohm-cm
1.50e+14
ohm-cm
60°C for 1,000 hrs with 90% RH
Dielectric Strength
5.00
kV/mm
127
kV/in
JIS-K-6249/ASTM D-149
Dielectric Breakdown
3000
V
3000
V
Withstand Voltage [V/min]; JIS-K-6249/ASTM D-149
Thermal Properties
Metric
English
Comments
Thermal Conductivity
1.50
W/m-K
10.4
BTU-in/hr-ft²-°F
150°C for 1,000 hrs; JIS-R-2618
1.50
W/m-K
10.4
BTU-in/hr-ft²-°F
60°C for 1,000 hrs with 90% RH; JIS-R-2618
1.50
W/m-K
10.4
BTU-in/hr-ft²-°F
70°C for 1,000 hrs; JIS-R-2618
Maximum Service Temperature, Air
150
°C
302
°F
Minimum Service Temperature, Air
-40.0
°C
-40.0
°F
Flammability, UL94
V-0
V-0
Descriptive Properties
Color
Dark Grey
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NeoGraf eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive
ITW Insulcast® RTVS 3-95-1 Silicone Potting/Encapsulation Compound
ITW Insulcast® RTVS 27 HTC Silicone Potting/Encapsulation Compound
Fujipoly Industries Sarcon® 45Q Thin-Film QR
Dow Sylgard® 3-6605 Thermally Conductive Silicone Elastomer
PFUJIP28 / 39161
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.