MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis KOBLEND PCA 447 PC+ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Symbol according to ISO 1043/1: PC+ABS

Injection moulding grade with very good impact behaviour even at low temperatures, good dimensional stability. Vicat/B50 = 110°C

Main application fields: automotive interiors, domestic appliances industry, electrical industry

Unfilled. Suitable for Injection Molding. Supplied as pellets.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Key Words: Poly(Acrylonitrile Butadiene Styrene) + Polycarbonate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Water Absorption 0.70 %0.70 %
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 260 °C
16 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm³/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi50 mm/min
Elongation at Break >= 50 %>= 50 %Nominal
Elongation at Yield 3.6 %3.6 %50 mm/min
Tensile Modulus 2.10 GPa305 ksi1 mm/min
Izod Impact, Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Izod Impact, Notched (ISO) 25.0 kJ/m²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
 2.8
@Frequency 100 Hz
2.8
@Frequency 100 Hz
Dielectric Strength 27.0 kV/mm686 kV/in
Dissipation Factor  0.0040
@Frequency 100 Hz
0.0040
@Frequency 100 Hz
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
Comparative Tracking Index 500 V500 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °F
Vicat Softening Point 114 °C237 °F50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo PULSE™ B-270 PC/ABS
Versalis KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber
Covestro Bayblend® FR3000 PC/ABS Blend
Edinburg Plastics CAI406 PC/ABS
Engineered Plastics EP Alloy 510G PC/ABS Alloy

PENJ13 / 35902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.