MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA951000 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processability, toughness and drawdown.

Regulatory Status
The basic resin NA 951 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing NA 951 can only be made when the processing conditions, equipment and end use are known.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 31.8 microns1.25 mil2:1 BUR; 25 mil die gap
Melt Flow 2.2 g/10 min2.2 g/10 minASTM D1238
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.6 MPa1970 psiMolded; ASTM D638
Film Elongation at Break, MD 250 %250 %ASTM D882
Film Elongation at Break, TD 520 %520 %ASTM D882
Elongation at Break 600 %600 %Molded; ASTM D638
Elmendorf Tear Strength MD 320 g320 gASTM D1922
Elmendorf Tear Strength TD 100 g100 gASTM D1922
Dart Drop Test 100 g0.221 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 24.8 MPa3600 psiASTM D882
Film Tensile Strength at Break, TD 17.2 MPa2500 psiASTM D882
1% Secant Modulus, MD 197 MPa28500 psiASTM D882
1% Secant Modulus, TD 228 MPa33000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 °C350 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade)
LyondellBasell Petrothene® LR734001 High Density Polyethylene, Sheet & Profile Extrusion Data
Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding
A. Schulman POLYFORT™ PP 3045
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded

PEQU0498 / 36959

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.