MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestodur® X7390 Heat Stabilized PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Description: VESTODUR X7190 and X7390 are unreinforced, heat-stabilized and polymer modified polybutylene terephthalate (PBT) compounds with low shrinkage for extrusion. The compounds are especially suitable for the manufacture of stiff, small diameter tubing, e.g., loose buffering for fiber optics. VESTODUR X7390 has increased hydrolysis and heat resistance. Compared with standard PBT compounds X7190 and X7390 are harder. Therefore, they can also be used to protect as outer sheaths to protect electrical cables from the chewing of rodents. Both compounds contain a processing aid which facilitates feeding in the extrusion process.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
@Thickness 2.00 mm
0.012 - 0.014 in/in
@Thickness 0.0787 in
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.012 - 0.014 cm/cm0.012 - 0.014 in/in
Melt Flow 10.24 g/10 min
@Load 2.16 kg,
Temperature 250 °C
10.24 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787ISO 868
Tensile Strength, Yield 61.0 MPa8850 psiISO 527-1/2
Elongation at Break >= 50 %>= 50 %ISO 527-1/2
Elongation at Yield 6.5 %6.5 %ISO 527-1/2
Tensile Modulus 2.40 GPa348 ksiISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.650 J/cm²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal; ISO 11359, DIN 53752
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359, DIN 53752
Vicat Softening Point 150 °C302 °FMethod B, 50 N; ISO 306
 210 °C410 °FMethod A, 10 N; ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 6550 L PBT
Evonik Vestodur® 3010 High Viscosity, Hydrolysis Resistant PBT
Evonik Vestodur® 3000 High Viscosity PBT
Evonik Vestodur® 2000 Medium Viscosity PBT
Envalior Pocan® DP CF 2200 000000 PBT+PC

PHUMA69 / 47583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.