MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoreLite BALSASUD® Core SG Standard Grade Balsa Core Material
Categories: Other Engineering Material; Composite Core Material; Polymer; Renewable/Recycled Polymer; Wood and Natural Products; Wood

Material Notes: BALSASUD® Core is an end-grain balsa wood core material, ideal for sandwich construction. It has remarkable physical properties, starting with its outstanding strength-to-weight ratios (high shear and compression strength). It is an all-natural and renewable resource.

Thicknesses available between 3/16" to 3". Standard length and width 24" x 48". Property data tested perpendicular to the plane.

Information provided by CoreLite.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.152 g/cc0.00550 lb/in³Nominal; ASTM C-271
 0.130 - 0.176 g/cc0.00469 - 0.00637 lb/in³Tolerance
Moisture Absorption at Equilibrium 6 - 12 %6 - 12 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 14.39 MPa2087 psiASTM C-297
Tensile Modulus 3.574 GPa518.4 ksiASTM C-297
Compressive Strength 10.67 MPa1548 psiASTM C-365
Compressive Modulus 2.349 GPa340.7 ksiASTM C-365
Shear Modulus 0.186 GPa27.0 ksiASTM C-273
Shear Strength 2.720 MPa394.5 psiASTM C-273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0663 W/m-K0.460 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 163 °C325 °F
Minimum Service Temperature, Air -212 °C-350 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carbon-Core Carbon Balsa Wood
DIAB ProBalsa® PB Standard Balsa Wood
CoreLite BALSASUD® Core HW Heavy Weight Balsa Core Material
CoreLite BALSASUD® Core UL Ultra Lite Balsa Core Material
DIAB ProBalsa® LD7 Light Weight Balsa Wood

PCOREL991 / 180623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.