MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Chlorosulfonated Polyethylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 - 1.70 g/cc0.0387 - 0.0614 lb/in³Average value: 1.24 g/cc Grade Count:20
pH 12.012.0Average value: 12.0 Grade Count:4
Viscosity 45.0 - 260 cP45.0 - 260 cPAverage value: 148 cP Grade Count:3
Mooney Viscosity 15.0 - 12015.0 - 120Average value: 52.8 Grade Count:45
Thickness 800 - 1590 microns31.5 - 62.5 milAverage value: 1330 microns Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 38.0 - 10538.0 - 105Average value: 70.5 Grade Count:58
Tensile Strength, Ultimate 6.00 - 31.8 MPa870 - 4610 psiAverage value: 17.3 MPa Grade Count:50
Tensile Strength, Yield 4.90 - 15.6 MPa711 - 2260 psiAverage value: 11.4 MPa Grade Count:10
Elongation at Break 50.0 - 800 %50.0 - 800 %Average value: 376 % Grade Count:50
 500 - 650 %
@Temperature 50.0 - 50.0 °C
500 - 650 %
@Temperature 122 - 122 °F
Average value: 575 % Grade Count:2
Resilience 55.0 - 75.055.0 - 75.0Average value: 63.1 Grade Count:12
Tear Strength Test 153 - 337153 - 337Average value: 271 Grade Count:8
Graves Tear Strength 28.0 - 220 kN/m160 - 1260 pliAverage value: 112 kN/m Grade Count:15
Compression Set 8.00 - 69.0 %8.00 - 69.0 %Average value: 35.5 % Grade Count:33
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 - 204 °C257 - 400 °FAverage value: 136 °C Grade Count:13
Minimum Service Temperature, Air -65.0 - -2.00 °C-85.0 - 28.4 °FAverage value: -37.1 °C Grade Count:29
Brittleness Temperature -65.0 - -2.00 °C-85.0 - 28.4 °FAverage value: -37.1 °C Grade Count:18
Clash Berg Stiffness Temperature -26.0 - 7.00 °C-14.8 - 44.6 °FAverage value: -17.6 °C Grade Count:15
Flash Point 260 °C500 °FAverage value: 260 °C Grade Count:10
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 24.0 - 41.0 %24.0 - 41.0 %Average value: 33.8 % Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Overview of materials for Silicone Rubber
Overview of materials for Thermoset Fluoroelastomer
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Polychloroprene Rubber (CR)

O5160 / 78472

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.