MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

MMCC Al/B4C Particulate Aluminum Matrix Composite  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.

Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).

MatWeb has no current information on Metal Matrix Cast Composites (MMCC).

Key Words: Aluminium; Boron Carbide B4C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.60 g/cc0.0939 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 300 - 400 MPa43500 - 58000 psi
Modulus of Elasticity 190 - 200 GPa27600 - 29000 ksiYoungs Modulus
Fracture Toughness 10.0 - 25.0 MPa-m½9.10 - 22.8 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 - 10.0 µm/m-°C
@Temperature 20.0 °C
4.44 - 5.56 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 75.0 W/m-K521 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MMCC Al/SiC Particulate Aluminum Matrix Composite
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite
MMCC Aluminum/SiC 55p Aluminum Matrix Composite
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite

NZMMB6 / 20032

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.