MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

5% Sn Antimonial Lead Solder, UNS L54321
Categories: Metal; Nonferrous Metal; Lead Alloy; Solder/Braze Alloy

Material Notes: Various specifications are possible for exact composition and impurity limits.

Key Words: Lead Alloys, ASTM B32 (5B)
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 11.3 g/cc0.408 lb/in³Calculated
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 88
Tensile Strength, Ultimate 28.0 MPa4060 psi
Elongation at Break 55 %55 %in 50 mm
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb 0.20 - 5.0 %0.20 - 5.0 %
Arsenic, As <= 0.020 %<= 0.020 %
Bismuth, Bi <= 0.25 %<= 0.25 %
Copper, Cu <= 0.080 %<= 0.080 %
Iron, Fe <= 0.020 %<= 0.020 %
Lead, Pb 95 %95 %
Tin, Sn 4.5 - 5.5 %4.5 - 5.5 %
Zinc, Zn <= 0.0050 %<= 0.0050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
5/95 Solder (95Pb-5Sn), UNS L54320
60-40 Soft Solder (60 Sn-40Pb) - ASTM B 32 Grade Sn60
In60-Pb40 Indium-Lead Solder
In50-Sn50 Indium-Tin Solder
In70-Pb30 Indium-Lead Solder

MLSS04 / 12255

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.