MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Finished product available as bar, wire, or rod.
Chicago Extruded Metal temper codes: H02, M30

This alloy is registered with the U.S. EPA as Antimicrobial.

Information provided by Chicago Extruded Metals

Key Words: CDA 647, ASTM B411, ASTM B412
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 552 - 621 MPa80000 - 90000 psi
Tensile Strength, Yield 483 - 517 MPa70000 - 75000 psi
Elongation at Break 8.0 %8.0 %
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 95.81 - 96.81 %95.81 - 96.81 %as balance
Iron, Fe 0.10 %0.10 %
Lead, Pb 0.090 %0.090 %
Nickel, Ni 1.6 - 2.2 %1.6 - 2.2 %
Other, total 0.50 %0.50 %
Silicon, Si 0.40 - 0.80 %0.40 - 0.80 %
Zinc, Zn 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Everdur, UNS C87300, Copper Casting Alloy
Chicago Extruded Metals BioBrass® UNS C95520 As-Cast Aluminum Bronze
Materion BrushBronze® 95510 (AMS 4880) Continuous Cast 4.0" - 17.0"
UNS C81100, Copper Casting Alloy
Low-silicon bronze B, UNS C65100, OSO35 Temper rod

NCHICA924 / 147643

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.