MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adhesive offers strong, durable, chemically and environmentally resistant bonds. Lord 309 adhesive has demonstrated excellent adhesion to prepared metals, FRP, wood, prepared rubber, and other materials.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.989 - 1.04 g/cc0.0357 - 0.0376 lb/in³309-2D Hardener
 1.26 - 1.29 g/cc0.0455 - 0.0466 lb/in³309-1D Resin
Solids Content 100 %100 %309-1D Resin
 100 %100 %309-2D Hardener
 100 %100 %Mixed
Water Absorption 0.21 %
@Time 86400 sec
0.21 %
@Time 24.0 hour
ASTM D570-81
Brookfield Viscosity  300000 - 1.00e+6 cP
@Temperature 25.0 °C
300000 - 1.00e+6 cP
@Temperature 77.0 °F
309-2D Hardener; HBF with Helipath and T-C @ 5rpm
 300000 - 1.00e+6 cP
@Temperature 25.0 °C
300000 - 1.00e+6 cP
@Temperature 77.0 °F
Mixed; HBF with Helipath and T-C @ 5rpm
 300000 - 1.10e+6 cP
@Temperature 25.0 °C
300000 - 1.10e+6 cP
@Temperature 77.0 °F
309-1D Resin; HBF with Helipath and T-C @ 5rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474Lord TM 23B
Tensile Strength at Break 37.9 MPa5500 psiASTM D882-83A (mod)
Elongation at Break 6.0 %6.0 %ASTM D882-83A (mod)
Modulus of Elasticity 1.086 GPa157.5 ksiASTM D882-83A (mod)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 268 µm/m-°C149 µin/in-°Fabove Tg; Lord Internal Method (by DMA)
Glass Transition Temp, Tg 70.0 °C158 °FASTM E1640-99 (by DMA)
Flash Point >= 93.0 °C>= 199 °F309-1D Resin; Closed Cup
 >= 93.0 °C>= 199 °F309-2D Hardener; Closed Cup
 >= 93.0 °C>= 199 °FMixed; Closed Cup
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 - 2880 min
@Temperature >=18.0 °C
24.0 - 48.0 hour
@Temperature >=64.4 °F
Pot Life 90 - 120 min
@Temperature 25.0 °C
90 - 120 min
@Temperature 77.0 °F
54g mass
Shelf Life  12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
309-1D Resin
 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
309-2D Hardener
 
Descriptive Properties
AppearanceAmber309-2D Hardener
 Blue309-1D Resin
 Blue-greenMixed
ConsistencyPaste309-1D Resin
 Paste309-2D Hardener
 PasteMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive

PLORD109 / 86117

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.