MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Krytox® 202 GPL Standard Grade Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE); PTFE Gellant

Material Notes: Krytox® GPL 200–207 greases are white buttery greases with all of the same properties as the GPL 100–107 oils that they are made from, but they are in grease form. The grease additives may alter the chemical resistance of the grease. The standard grease consistency is NLGI grade 2 penetration (265–295). Softer or harder NLGI penetration grades can be made by special order. Special nonmelting silica thickeners are available for applications that are higher than the 325°C (617°F) melting point of the standard PTFE thickener. All standard grades of grease are thickened with Krytox® 2000 polytetrafluoroethylene (PTFE), whose formula is (CF2-CF2)n. This special high efficiency thickener has a melting point of 325°C (617°F) and has low molecular weight and submicron (0.2 m) particle size for higher performance in bearings.

Krytox® GPL 100–107 oils are clear, colorless, fluorinated synthetic oils that are nonreactive, nonflammable, safe in chemical and oxygen service, and are long-lasting. Krytox® is a perfluoropolyether (PFPE)—also called perfluoro-alkylether (PFAE) or perfluoropolyalkylether (PFPAE). The polymer chain is completely saturated and contains only carbon, oxygen, and fluorine. On a weight basis, a typical Krytox® oil contains 21.6% carbon, 9.4% oxygen, and 69.0% fluorine.

Information provided by DuPont Performance Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.72 g/cc
@Temperature 100 °C
0.0621 lb/in³
@Temperature 212 °F
 1.91 g/cc
@Temperature 0.000 °C
0.0690 lb/in³
@Temperature 32.0 °F
Viscosity Measurement 2929ASTM D2270
Kinematic Viscosity 38 cSt
@Temperature 20.0 °C
38 cSt
@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 15 cSt15 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.0 cSt3.0 cStASTM D445
Evaporation Loss 2.0 %2.0 %Volatility; 22 hr; 66°C; ASTM D972 Modified
 20 %
@Temperature 121 °C,
Time 79200 sec
20 %
@Temperature 250 °F,
Time 22.0 hour
Volatility; ASTM D972 Modified
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction, Dynamic 0.0700.0704-Ball Wear Test; 1200 rpm/60 min; ASTM D4172
Four Ball Wear 0.400 mm0.0157 in1200 rpm/60 min; ASTM D4172
Falex Load Test 567000 g1250 lbV-Block Load Carrying Ability; 32 in-lb torque at max load; ASTM D3233
Oil Separation 7.0 %7.0 %30 hr; 99°C; FTMS 791B 321.1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 132 °C270 °F
Minimum Service Temperature, Air -63.0 °C-81.4 °F
Pour Point -63.0 °C-81.4 °FASTM D97
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 21.6 %21.6 %
Fluorine, F 69 %69 %
Oxygen, O 9.4 %9.4 %
 
Descriptive Properties
ISO Grade of Oil15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Krytox® 214 GPL Extreme Pressure Grease
Chemours Krytox® 16256 Vacuum Pump Fluid
Chemours Krytox® 1531XP Vacuum Pump Fluid with Antirust Protection
Chemours Krytox® 1531 Vacuum Pump Fluid
Chemours Krytox® 1525XP Vacuum Pump Fluid with Antirust Protection

WDUPK33 / 75393

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.