MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Geniosil® GF 95 Silane
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C8H22N2O2Si

CAS No.: 3069-29-2

Properties: The use of GENIOSIL® GF 95 as an adhesion promoter in glassfiber reinforced or filler modified plastics increases filler dispersibility and improves numerous mechanical properties (e.g. flexural strength, tensile strength, modulus of elasticity) of the composites. Additionally, its use reduces the fillers' sedimentation tendency in the uncured polymer. The use of GENIOSIL® GF 95 in these materials also results in a markedly improved resistance to water (vapor) and corrosion. At the same time, the mechanical properties can be adjusted with even greater precision by means of the dialkoxysilyl group. As textile finishing agents, Silicones modified with GENIOSIL® GF 95 result in amino modified silicone fluids that are an ideal active ingredient in softener formulations for finishing fibers and textiles.

Special features: GENIOSIL® GF 95 is an alkoxysilane with an amino functional group. It´s a clear, colorless liquid with a characteristic amine odor. Due to the nature of the amino group, this substance reacts as a base. The silane hydrolyzes auto catalytically in the presence of moisture (methanol is released) to form silanols, which can subsequently react with themselves to produce siloxanes or can bind to inorganic substrates. As a bifunctional amine, GENIOSIL® GF 95 can also interact with numerous organic polymers and thus function as a molecular bridge between organic and inorganic substrates. An additional bonus deriving from the dialkoxysilyl group in GENIOSIL® GF 95 is that VOC (volatile organic compound) emissions during hydrolysis reactions are reduced by one third compared to trialkoxysilanes.

Application: GENIOSIL® GF 95 is mainly used in glass-fiber or glass-fabric reinforced polyesters and polyolefin molded parts, and as a surface modifier for fillers (e.g. glass or mineral wool, mica, talc, wollastonite, kaolin, christobalite, metal oxides) and pigments for various plastics, including epoxy resins, polyamides, polyacrylates, polyurethanes, ethylene/vinyl acetate polymers and many others. Other important applications include its uses as a silicone modifying building block for textile finishing and as an additive or primer for sealants, adhesives and coatings.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³DIN 51757
Viscosity 4.7 cP4.7 cPdynamic; DIN 51562
Molecular Weight 206.4 g/mol206.4 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point 110 °C
@Pressure 0.000300 MPa
230 °F
@Pressure 0.0435 psi
Flash Point >= 100 °C>= 212 °FISO 2719
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4471.447
 
Descriptive Properties
Amine number9.4 percent
Purity>95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo INSPIRE™ DLGF 9621.00 Compounded Polypropylene, 60% LGF
Wacker Geniosil® GF 91 Silane
Trinseo INSPIRE™ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF
Silon Tabond 5007 Adhesive Resin
Silon Tabond 3021 Adhesive Resin

PWACK9321 / 204850

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.