MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco 141 Refined Wax
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Refined Waxes are fully refined, food grade waxes meeting the highest purity standards. Derived from petroleum using a solvent refining process, Chevron Refined Waxes are comprised of a mixture of normal paraffins ranging in carbon number from 20 to 43.

Chevron Refined Waxes are available in two melting point grades. When heated, these waxes melt to become colorless, low viscosity liquids with low odor. When cooled, they harden to become opaque, semi crystalline solids.

In addition to their well-defined melting points, each grade offers an array of functional properties that determine its suitability for a given application.

  • Important solid-phase properties include water repellency, hardness, surface adhesion, visual aesthetic (e.g. gloss), low temperature flexibility, and resistance to blocking.
  • Important liquid-phase properties include viscosity, solubility and emulsibility.
All Chevron Refined Waxes comply with the following U.S. Food and Drug Administration (FDA) regulations pertaining to the use of petroleum wax in, on or in contact with food:
  • 21 CFR 172.886 – use as a food additive permitted fro direct addition to food
  • 21 CFR 178.3710 – use as a component of nonfood articles in contact with food.
  • 21 CFR 176.170 and 21 CFR 176.180 – use as a component of paper and paperboard in contact with aqueous and fatty foods; and dry foods, respectively.
Chevron Refined Waxes also comply with a host of other regulations including:
  • Coalition of Northeastern Governors (CONEG) Model Toxic Legislation banning the use of heavy metals in packaging materials.
  • State of California Proposition 65 regulating exposure to and warnings regarding chemicals known to the state to cause cancer and reproductive toxicity.
  • Federal Clean Air Act of 1990 regulating the atmospheric emission of volatile organic hydrocarbons.

Applications

Chevron Refined Waxes offer outstanding value and performance in a wide range of packaging and nonpackaging applications including :

  • Packaging Applications – Coatings for:
    • Flexible paper packaging
    • Folding Cartons
    • Corrugated boxes
    • Paper cups
    • Waxed paper
  • Nonpackaging Application
    • Candies
    • Cheese, fruit and vegetable coatings
    • Cosmetics
    • Crayons
    • Hot melt adhesives
    • Metalworking fluid additives
    • Pharmaceuticals
    • Polishes and waxes
    • PVC lubricants
    • Tire and rubber antiozonants

Key Words: CPS Number: 261004; MSDS Number: 7322
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.7708 g/cc
@Temperature 82.2 °C
0.02785 lb/in³
@Temperature 180 °F
ASTM D4052
Kinematic Viscosity at 100°C (212°F) 4.3 cSt4.3 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Penetration  13
@Thickness 0.100 mm,
Temperature 25.0 °C
13
@Thickness 0.00394 in,
Temperature 77.0 °F
 40 - 65
@Thickness 0.100 mm,
Temperature 37.8 °C
40 - 65
@Thickness 0.00394 in,
Temperature 100 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 58.3 °C137 °F
Flash Point 450 °C842 °FASTM D92
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Blocking Point, °F114
Color+29, Saybolt
Oil Content wt%0.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco 128 Refined Wax
ChevronTexaco Saturating Wax 2
Michelman® Michem® Emulsion 80939M Nonionic paraffin wax emulsion
Michelman® Michem® Emulsion 91840 Nonionic HD polyethylene / paraffin wax emulsion
Michelman® FiberMax® 5000 Water based medium treatment to replace paraffin wax

WCHEV386 / 75001

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.