LNP Thermocomp® RF-1008 Polyamide 66, Glass Fiber Reinforcement
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
Material Notes:
Forms: Pellets
Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.47
g/cc
1.47
g/cc
Method A; ASTM D792
Water Absorption
0.60 %
0.60 %
at 24 hrs; ASTM D570
Linear Mold Shrinkage
0.0030
cm/cm
0.0030
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.013
cm/cm
0.013
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
184
MPa
26700
psi
ASTM D638
Tensile Strength, Yield
184
MPa
26700
psi
ASTM D638
Elongation at Break
2.5 %
2.5 %
ASTM D638
Elongation at Yield
2.5 %
2.5 %
ASTM D638
Tensile Modulus
13.3
GPa
1930
ksi
ASTM D638
Flexural Strength
269
MPa
39000
psi
ASTM D790
Flexural Modulus
10.4
GPa
1510
ksi
ASTM D790
Izod Impact, Notched
1.17
J/cm
@Thickness 3.18 mm
2.19
ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched
11.4
J/cm
@Thickness 3.18 mm
21.4
ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO)
13.1
kJ/m²
6.23
ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO)
74.0
kJ/m²
35.2
ft-lb/in²
ISO 180
Falling Dart Impact
10.3
J
7.60
ft-lb
ASTM D3763
Instrumented Impact Total Energy
3.08
J
2.27
ft-lb
Multi-Axial Instrumented Impact Energy; ISO 6603-2
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
253
°C
487
°F
Unannealed; ASTM D648
Flammability, UL94
HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Processing Properties
Metric
English
Comments
Melt Temperature
282
-
302
°C
540
-
576
°F
Mold Temperature
93.3
-
107
°C
200
-
225
°F
Drying Temperature
82.2
°C
180
°F
Dry Time
4
hour
4
hour
Moisture Content
0.20 %
0.20 %
Suggested
Back Pressure
0.172
-
0.345
MPa
24.9
-
50.0
psi
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LNP Thermocomp® OF-1008 Polyphenylene Sulfide, Glass Fiber Reinforcement
LNP Thermocomp® RF-1008 HS BK8-115 Polyamide 66, Glass Fiber Reinforcement
LNP Thermocomp® RF-1008 EM HS Polyamide 66, Glass Fiber Reinforcement
Radici Radilon® ARV300 RKC (dry) Nylon 66
Radici Radilon® A RV400 (dry) Nylon 66
PZLNP1518 / 51600
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.