MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3M Scotchkote™ EG 503 Epoxy Metal Repair
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Metal Repair EG 503 is a specifically developed high performance metal compound that provides good mechanical strength combined with easy machining properties.

Product Features:

  • Combines good machining characteristics with good mechanical properties
  • Designed for application by trowel or spatula at thicknesses up to 12 mm
  • Provides outstanding cold weld capabilities
  • Designed for use to repairs to cracked casting and rebuilding worn shafts, bearing housings and flanges
  • Excellent adhesion to correctly prepared metal surface.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Thickness 11900 microns470 mil
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 68.9 MPa10000 psi
Compressive Strength 107 MPa15500 psi
Shear Strength 17.2 MPa2500 psiTensile Shear Adhesion
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 90.0 °C194 °Fpost cured 24 hrs at 100°C
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourInitial Set
 4320 min72.0 hourFull Cure
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchkote™ SG 527 Epoxy Metal Repair
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste
Overview of materials for Epoxy, Cast, Metal Filled
Polynt DISTITRON® VE 100 ST Epoxy Resin Based Vinyl Ester
Polynt EPOVIA OPTIMUM® KRF 1001 TAS Bisphenol-A Epoxy Resin

PMM35297 / 170044

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.