MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 5454-H111; 5454-H311
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: AA5454-H11; AA5454-H311, UNS A95454; ISO AlMg3Mn; Aluminum 5454-H311; Aluminium 5454-H111, Aluminium 5454-H311; Al5454-H111
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.69 g/cc0.0972 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 9393Converted from Brinell Hardness Value
Hardness, Vickers 8080Converted from Brinell Hardness Value
Tensile Strength, Ultimate 262 MPa38000 psiAA; Typical
Tensile Strength, Yield 179 MPa26000 psiAA; Typical
Elongation at Break 14 %
@Thickness 1.59 mm
14 %
@Thickness 0.0625 in
AA; Typical
Modulus of Elasticity 70.3 GPa10200 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 159 MPa23000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000510 ohm-cm0.00000510 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.9 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.2 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 23.7 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
 24.6 µm/m-°C
@Temperature 20.0 - 200 °C
13.7 µin/in-°F
@Temperature 68.0 - 392 °F
 25.6 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 134 W/m-K930 BTU-in/hr-ft²-°F
Melting Point 601.7 - 646.1 °C1115 - 1195 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 601.7 °C1115 °FAA; Typical
Liquidus 646.1 °C1195 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °Fholding at temperature not required
Hot-Working Temperature 260 - 510 °C500 - 950 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 94.4 - 97.1 %94.4 - 97.1 %As remainder
Chromium, Cr 0.05 - 0.20 %0.05 - 0.20 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 2.4 - 3.0 %2.4 - 3.0 %
Manganese, Mn 0.50 - 1.0 %0.50 - 1.0 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5083-H116; 5083-H321
Aluminum 6061-T6; 6061-T651
Aluminum 5454-O
Aluminum 5083-H112
Aluminum 5052-O

MA5454H111 / 9276

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.