MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® XE 3841 nat PA12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe for direct contact with foodstuffs and alcoholic beverages. The main features of Grilamid XE 3841 are:
  • Plasticizer free
  • Very flexible
  • Translucent
  • Good low temperature impact strength
  • Low density
Grilamid XE 3841 is suitable for use on Tubes used in the food preparation industry as well as pneumatic tubes.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³Dry; ISO 1183
Water Absorption 1.1 %1.1 %Sim. to ISO 62
Moisture Absorption 0.600 %0.600 %Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 53
@Time 15.0 sec
53
@Time 0.00417 hour
Conditioned; ISO 868
Tensile Strength at Break 30.0 MPa4350 psiConditioned; ISO 527-1/-2
Tensile Strength, Yield 20.0 MPa2900 psiConditioned; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 15 %15 %Conditioned; ISO 527-1/-2
Tensile Modulus 0.350 GPa50.8 ksiConditioned; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 43.0 kV/mm1090 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 575 V575 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C88.9 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 100 °C176 - 212 °FLong Term; ISO 2578
 130 °C266 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °C113 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C104 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
ProcessingOther Extrusion
Product AttributesFlexible
Special CharacteristicsHigh impact or impact modified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsamid® AECV BLACK T8L PA12
EMS-Grivory Grilamid® LC-15H black PA12-CF15
EMS-Grivory Grilamid® LC-3H black PA12-CF30
EMS-Grivory Grilamid® LV-23H PA12-GF23
EMS-Grivory Grilamid® XE 4129 black 9020 PA610

PGRH113 / 156822

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.