MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corbion Purac Blend C High Heat, Impact Modified Homopolymer PLA
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Increased impact is produced by addition of impact modifier to the base grade; a small amount of talc is added to preserve the modulus. Data is for samples produced from Puralact L and D lactide monomers. PLA is 100% biobased and is both recyclable and compostable. PLA can be used in a broad range of applications from molded plastic parts to textiles, foams, and films.

Information provide by Corbion Purac.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psi
Elongation at Break 60 %60 %
Tensile Modulus 3.50 GPa508 ksi
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FHDT B flatwise
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 220 °C374 - 428 °Fpre-drying required
Mold Temperature 70.0 - 100 °C158 - 212 °F
 
Descriptive Properties
ClarityNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corbion Purac Blend A High Heat Homopolymer PLA
Corbion Purac Blend B High Heat, High Modulus Homopolymer PLA
Overview of materials for Thermoset Polyurethane, Adhesive
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer
Overview of materials for Polylactic Acid (PLA) Biopolymer

PPURAC92 / 133274

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.