MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

H.C. Starck Amperit® 568.005 Tungsten Carbide-Nickel 92-8 - Nickel SF RC 60 65-35
Categories: Ceramic; Carbide

Material Notes: Composition is of NiSF RC 60 only

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 32 µm32 µmMaximum of 7% less than, WSC-Ni 92/8
 38 µm38 µmMaximum of 5% less than, Ni-SF RC 60
 45 µm45 µmMaximum of 20% less than, Ni-SF RC 60
 75 µm75 µmMaximum of 5% greater than, Ni-SF RC 60
 106 µm106 µmMaximum of 1% greater than, WSC-Ni 92/8
 
Component Elements PropertiesMetricEnglishComments
Boron, B 3.0 - 3.9 %3.0 - 3.9 %
Carbon, C 0.70 - 0.90 %0.70 - 0.90 %
Chromium, Cr 14.2 - 16.5 %14.2 - 16.5 %
Iron, Fe 3.5 - 4.5 %3.5 - 4.5 %
Nickel, Ni 69.4 - 74.6 %69.4 - 74.6 %
Silicon, Si 4.0 - 4.8 %4.0 - 4.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
H.C. Starck Amperit® 568.062 Tungsten Carbide-Nickel 92-8 - Nickel SF RC 60 65-35
3M Techical Ceramics EKagrip® 10 Friction-enhancing electroless nickel diamond coating
Chromium Carbide, Cr3C2
H.C. Starck Amperit® 413.3 Gas Atomized (NiCoCrAlY)

CHCSTA129 / 1307

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.