MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem GM7746C HDPE Blow Molding Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: GM7746C is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tenacity, high resistance to stress cracking, and outstanding impact resistance. Its applications include: mono and multilayer fuel tanks for automobiles, small volume automotive reservoirs, and sheet extrusion for pickup rear protectors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM-D792
ESCR 100% Igepal® >= 1000 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
>= 1000 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 4.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
4.5 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM-D2240
Tensile Strength at Break 42.0 MPa6090 psiASTM-D638
Tensile Strength, Yield 23.0 MPa3340 psiASTM-D638
Elongation at Break 880 %880 %ASTM-D638
Elongation at Yield 13 %13 %ASTM-D638
Flexural Modulus, 1% Secant 890 MPa129000 psiASTM-D790
Izod Impact, Notched 7.60 J/cm14.2 ft-lb/inASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM-D648
Vicat Softening Point 126 °C
@Load 1.02 kg
259 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
Braskem BU 004 HDPE Blow Molding Polyethylene
Borealis BB2581 HDPE for Blow Molding
Borealis BS2581 High Density Polyethylene for Blow Molding
Braskem BU004 Blow Molding High Density Polyethylene

PBRAS806 / 106652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.