MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGOMER® D 3403 Comonomer
Categories: Other Engineering Material

Material Notes: Product description: Due to its two hydroxyl groups TEGOMER® D 3403 may be used as a comonomer for the production of polyester and polyurethanes. Depending on the EO/PO ratio the resulting polymer will be more hydrophilic or better soluble in organic solvents. TEGOMER® D 3403 is specifically purified for the conversation with isocyanates. TEGOMER® D 3403 is miscible with water and most organic solvents like glycols, ethanol, chloroform, acetone, toluene and xylene. It is not miscible with paraffines.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 1200 g/mol1200 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 1.0<= 1.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 38.0 - 42.0 °C100 - 108 °F
 
Descriptive Properties
Appearancesolid
Hydroxyl Number85-99 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGOMER® PP-Si 401 Additive
Evonik TEGOMER® P 121 Dispersing additive

PEVONIL576 / 196780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.