MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis HD905CF Polypropylene Homopolymer for Cast Film
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: HD905CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, suitable for the manufacturing of unoriented film on chill roll process. It is recommended to use rather high chill roll temperatures in the range of 40-55°C to obtain the optimum film stiffness. Optical properties will not be deteriorated as with conventional homopolymers at these temperatures.

HD905CF is especially suitable for twist films, labeling films, lamination films, furniture films, decorating films, and textile films.

Former trade name for this product was Bormod™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.910 g/cc0.0325 - 0.0329 lb/in³ISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 80 %80 %ISO 527-3
Film Elongation at Break, TD 120 %120 %ISO 527-3
Flexural Modulus 2.10 GPa305 ksiISO 178
Secant Modulus, MD 1.60 GPa232 ksiISO 527-3
Secant Modulus, TD 1.80 GPa261 ksiISO 527-3
Impact 4040Dynatest, Damaging Force (N); ISO 7765-2
Impact Test 0.950 J0.701 ft-lbDynatest, Penetration Energy; ISO 7765-2
Coefficient of Friction 0.30 - 0.400.30 - 0.40Film/Film; ISO 8295
Film Tensile Strength at Break, MD 35.0 - 55.0 MPa5080 - 7980 psiISO 527-3
Film Tensile Strength at Break, TD 30.0 - 50.0 MPa4350 - 7250 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 164 - 170 °C327 - 338 °FISO 3146
Vicat Softening Point 158 °C316 °FA (10 N); ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 6.0 %<= 6.0 %ASTM D1003
Gloss >= 90 %>= 90 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem H 510 Bioriented Film Polypropylene
Borealis Daplen™ ED206HP TPO Compound
Formosa Plastics Formolene® 5144L Homopolymer Polypropylene
Ineos H07B-01 Polypropylene Homopolymer
LyondellBasell Adstif HA 748L Polypropylene

PBOREA087 / 27394

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.