Product Description: ExxonMobil™ C4LL 50026pw.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of ExxonMobil™ C4LL 50026pw.09 makes for efficient blending with pigments, slip additives, and antiblock additives. Availability: Latin America and North America Additive: - Antiblock: No
- Slip: No
- Processing Aid: No
- Thermal Stabilizer: Yes
Applications: Information provided by ExxonMobil |