MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Glass Reinforced, Impact Grade

Material Notes: SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in combination with low creep properties.

Information provided by SAX Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Viscosity Test 150 cm³/g1.50 dl/gH2SO4; ISO 307
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 120 MPa17400 psi5 mm/min; ISO 527-1
Elongation at Break 3.5 %3.5 %5 mm/min; ISO 527-1
Tensile Modulus 7.20 GPa1040 ksi1 mm/min; ISO 527-1
Flexural Strength 183 MPa26500 psi2 mm/min; ISO 178
Flexural Modulus 6.20 GPa899 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 21.0 kJ/m²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  90.0 kJ/m²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
 95.0 kJ/m²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1U
Charpy Impact Unnotched  8.30 J/cm²
@Temperature 23.0 °C
39.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 8.70 J/cm²
@Temperature -30.0 °C
41.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 237 °C459 °F80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 228 °C442 °FB/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 300 °C518 - 572 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C
@Time 7200 - 21600 sec
176 °F
@Time 2.00 - 6.00 hour
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66

PSAXP962 / 150911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.