MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ TF 1620 PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Meets ASTM D4894 Type IV, Grade 2 resin
  • Semi-free-flowing compression molding powder
  • High bulk density
  • Good for large billets and thin walled isostatic moldings
  • Very dense polymer structure, similar to non-free-flowing grades
  • Excellent flex life
  • Good dielectric strength

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc
@Temperature 23.0 °C
2.15 g/cc
@Temperature 73.4 °F
Sintering Molding; ASTM D4894-98a
Bulk Density 0.850 g/cc0.0307 lb/in³ASTM D4894-98a
Particle Size 220 µm220 µmaverage; ASTM D4894-98a
Deformation 11 %11 %2175 psi - permanent, 23°C, Sintering Molding; ASTM D621
 15 %15 %2175 psi - 24 hrs, 23°C, Sintering Molding; ASTM D621
 17 %17 %2175 psi - 100 hrs, 23°C, Sintering Molding; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 27.58 MPa>= 4000 psiSintered Molding; ASTM D4894-98a
Elongation at Break 350 %350 %Sintered Molding; ASTM D4894-98a
Tensile Modulus 0.600 GPa87.0 ksiSintered Molding; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 2.50 kV/mm63.5 kV/inASTM D149-95a
 
Thermal PropertiesMetricEnglishComments
Melting Point 317 - 337 °C603 - 639 °Fsecond; ASTM D4894-98a
 332 - 352 °C630 - 666 °Finitial; ASTM D4894-98a
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -200 °C-330 °F
Flammability, UL94 V-0V-0
Shrinkage 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
Sintering Moldings; ASTM D4894-98a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ TF 1641 PTFE
3M Dyneon™ TF 1645 PTFE
3M Dyneon™ TF 1750 PTFE
3M Dyneon™ TFM™ 1600 PTFE
3M Dyneon™ TF 5050Z PTFE

PDYNE030 / 34838

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.