MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Hexcel designation: 7781-38"-F515; Fiber 75-1/0

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  414 MPa
@Temperature 71.0 °C
60000 psi
@Temperature 160 °F
1/2 hr
 483 MPa
@Temperature 23.0 °C
70100 psi
@Temperature 73.4 °F
Tensile Modulus  27.6 GPa
@Temperature 71.0 °C
4000 ksi
@Temperature 160 °F
1/2 hr
 30.3 GPa
@Temperature 23.0 °C
4390 ksi
@Temperature 73.4 °F
Flexural Yield Strength  483 MPa
@Temperature 71.0 °C
70100 psi
@Temperature 160 °F
1/2 hr
 621 MPa
@Temperature 23.0 °C
90100 psi
@Temperature 73.4 °F
Flexural Modulus  22.1 GPa
@Temperature 71.0 °C
3210 ksi
@Temperature 160 °F
1/2 hr
 23.4 GPa
@Temperature 23.0 °C
3390 ksi
@Temperature 73.4 °F
Compressive Yield Strength  276 MPa
@Temperature 71.0 °C
40000 psi
@Temperature 160 °F
1/2 hr
 414 MPa
@Temperature 23.0 °C
60000 psi
@Temperature 73.4 °F
Compressive Modulus  21.4 GPa
@Temperature 71.0 °C
3100 ksi
@Temperature 160 °F
1/2 hr
 27.6 GPa
@Temperature 23.0 °C
4000 ksi
@Temperature 73.4 °F
Shear Strength 24.8 MPa
@Temperature 23.0 °C
3600 psi
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric
Hexcel® HexForce™ 7781 Fiber Glass Fabric
E-Glass Fiber, Generic
Fibre Glast 543 Style 7781 E-Glass Fiberglass Fabric
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric

PHEXC132 / 98602

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.