MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Applications:
  • Coiled bobbins
  • Mouthpieces
Features:
  • High cycles

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³ASTM D792
Water Absorption 0.060 %0.060 %ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inMD
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ASTM D785
Tensile Strength at Break 100 MPa14500 psiASTM D638
Elongation at Break 2.2 %2.2 %ASTM D638
Flexural Strength 145 MPa21000 psiASTM D790
Flexural Modulus 7.10 GPa1030 ksiASTM D790
Izod Impact, Notched 0.570 J/cm1.07 ft-lb/inASTM D256
Taber Abrasion, mg/1000 Cycles 3535CS-17; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
ASTM D149
Arc Resistance 139 sec139 secUL recognition value, tungsten electrode; ASTM D495
Comparative Tracking Index 250 - 399 V250 - 399 VIEC Pub1.112, class 2; IEC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature 20.0 °C
22.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 255 °C491 °FBy DSC
Maximum Service Temperature, Air 120 °C248 °FThermal index; ASTM UL746B
 225 °C437 °FBall pressure temperature; IEC Method
Deflection Temperature at 0.46 MPa (66 psi) 240 °C464 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FASTM D648
Flammability, UL94 HB
@Thickness 0.7937 mm
HB
@Thickness 0.03125 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 255 - 265 °C491 - 509 °F
Mold Temperature 90.0 - 120 °C194 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced
Indorama AlphaPet Preformance® 1708CC(A) PET Resin
Hippe PET Polyethylene Terephthalate
Asahi Kasei Xyron™ AG213 PA/PPE

PTOY649 / 70809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.