MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Haynes CABVAL Hastelloy® G-50™ Grade 125 Ni-Cr-Fe-Mo Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Developed as a lower cost alternative to Hastelloy C-276 for use by producers of sour gas. Improved corrosion resistance compared to G-3 in service with high hydrogen disulfide concentrations in combination with carbon dioxide, chloride, etc. Its corrosion resistance at elevated temperatures falls between G-3 and C-276 in 15% HCl and in hydrogen sulfide stress corrosion cracking tests. G-50 alloy lends itself to consistent methods of manufacture of tubular products.

Data provided by CABVAL, a joint venture between Haynes International and Vallourec Industries.

Key Words: UNS N06950
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.33 g/cc0.301 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 313313Estimated from Rockwell C for Brinell 10 mm ball/3000 kg load
Hardness, Knoop 372372Estimated from Rockwell C
Hardness, Rockwell A 67.567.5Estimated from Rockwell C
Hardness, Rockwell C <= 34<= 34
Hardness, Vickers 326326Estimated from Rockwell C
Tensile Strength, Ultimate >= 900 MPa>= 131000 psi
Tensile Strength, Yield 860 - 1000 MPa
@Strain 0.2 %
125000 - 145000 psi
@Strain 0.2 %
Elongation at Break >= 13 %>= 13 %
Modulus of Elasticity 192 GPa
@Temperature 23.0 °C
27800 ksi
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.0 µm/m-°C
@Temperature 20.0 - 95.0 °C
7.22 µin/in-°F
@Temperature 68.0 - 203 °F
 13.54 µm/m-°C
@Temperature 20.0 - 204 °C
7.522 µin/in-°F
@Temperature 68.0 - 399 °F
 14.09 µm/m-°C
@Temperature 20.0 - 315 °C
7.828 µin/in-°F
@Temperature 68.0 - 599 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.40 %<= 0.40 %
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 19 - 21 %19 - 21 %
Cobalt, Co <= 2.5 %<= 2.5 %
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe 15 - 20 %15 - 20 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 8.0 - 10 %8.0 - 10 %
Nickel, Ni >= 50 %>= 50 %
Niobium, Nb (Columbium, Cb) <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.015 %<= 0.015 %
Tungsten, W <= 1.0 %<= 1.0 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes CABVAL Hastelloy® G-50™ Grade 100 Ni-Cr-Fe-Mo Alloy
Haynes CABVAL Hastelloy® G-50™ Grade 140 Ni-Cr-Fe-Mo Alloy
Haynes CABVAL Hastelloy® G-50™ Grade 110 Ni-Cr-Fe-Mo Alloy
Carlson C 600ESR Nickel-Chromium-Iron Alloy
Carlson C 600 Nickel-Chromium-Iron Alloy

NHAG52 / 16789

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.