MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Duracon® SF-15 Acetal Co-polymer (POM), High impact, Flexible
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.

The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O) and carbon-carbon (-C-C- bond) comonomer groups are incorporated into its main chain. Therefore the copolymer has superior chemical and thermal stability, compared with acetal homopolymer.

Acetal co-polymer is well-balanced in terms of mechanical, chemical and thermal properties, and its superior moldability allows it to be widely employed in various industrial fields.

Information provided by PolyPlastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 38.0 MPa5510 psiISO 527-1, 2
Elongation at Break 100 %100 %ISO 527-1, 2
Tensile Modulus 1.70 GPa247 ksiISO 527-1, 2
Flexural Strength 51.0 MPa7400 psiISO 178
Flexural Modulus 1.50 GPa218 ksiISO 178
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+13 ohm-cm3.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 130 µm/m-°C
@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FISO 75-1, 2
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible
Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible
Celanese Hostaform® S 27076 Elastomer Modified Acetal Copolymer
KEP Kepital® TE-25 (FU2025) Acetal Copolymer, High toughness
Kolon KOCETAL® UR302 Toughened Grade Acetal Resin

PPOLPL027 / 57020

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.