Base Polymer: Polycarbonate Filler/Additive System: Special filler Special Features: High light diffusion, UV stabilized, good flow Market Segment: Automotive, Lighting Application Area: Lighting, light transparent components Typical Application: Display elements, operating elements, lamp covers Information provided by Albis Plastics |